Residual Heat Blackening · RHB

Blacken your parts with the heat they already carry.

RHB is a waterborne blackening agent for ferrous parts. You dip straight from the tempering furnace, hold 30 to 60 seconds, and the workpiece heat does the film formation. No 140 °C caustic blackening tank. No preheating. No acid pickle. No rinse stage.

200–560 °Cpart entry temperature
30–60 simmersion time
40–60 °Cbath temperature
1 : 10dilution with water

The cost of the conventional route

Every step you remove is a step you stop paying for

Hot black oxide works, and it has been the standard for a century. It also asks for a caustic bath at roughly 140 °C, preheated and dried parts, an acid pickle upstream, and rinsing downstream. If your parts are already leaving a tempering furnace at several hundred degrees, most of that is work you are doing twice.

Process stepHot black oxide (≈140 °C)RHB
Caustic blackening bathRequiredNot used
Preheat / dry parts before the bathRequiredNot used — the part arrives hot
Acid pickle upstreamTypicalNot used
Rinse after the bathRequiredNot used
Hydrogen embrittlement riskPresent with acid picklingNo acid, no electrolysis
Spent bathHot caustic, regulated effluentNear-neutral
Drying / curing after the bath—80–120 °C forced air (RHB-500)

RHB is not a drop-in for every shop. It needs parts that are genuinely hot when they reach the bath. Where there is no residual heat, the process does not apply.

How it runs

Four steps, and one of them is the furnace you already run

1

Degrease

Clean the parts and rinse to pH below 8.5. Oil left on the surface is the most common reason a film comes out patchy.

2

Temper

Run your normal tempering cycle. The parts leave the furnace at 200–560 °C for RHB-500, or 200–500 °C for RHB-3270.

3

Dip

Immerse straight into the bath at 40–60 °C for 30–60 seconds. Water flashes off on contact with the hot part.

4

Dry and oil

Cure at 80–120 °C in forced air for RHB-500, or 180–200 °C for 3–5 minutes for RHB-3270. Apply rust-preventive oil while warm.

A note on honest limits. RHB removes the blackening bath, the preheat, the pickle and the rinse. It does not remove drying. RHB-500 still needs 80–120 °C forced-air curing; RHB-3270 needs 180–200 °C for 3–5 minutes. Shops without a drying oven cannot run either grade, and we would rather say so now than after the first pallet.

Two grades

Choose by your salt spray requirement and your oven

The two grades share the same chemistry and differ in two measurable ways: the salt spray resistance of the unlubricated film, and the curing temperature the film needs.

PropertyRHB-500RHB-3270
FormConcentrate, waterborne emulsionConcentrate, waterborne emulsion
Solids content22 %22 %
pH as supplied (25 °C)88
Dilution, concentrate : water1 : 10 or leaner1 : 10 or leaner
Water qualityTap water acceptableDeionised, conductivity < 200 µS/cm
Part entry temperature200–560 °C
392–1040 °F
200–500 °C
392–932 °F
Bath temperature40–60 °C
104–140 °F
40–60 °C
104–140 °F
Immersion time30–60 s30–60 s
Drying / curing80–120 °C
176–248 °F, forced air
180–200 °C
356–392 °F, 3–5 min
Post-treatmentRust-preventive oilRust-preventive oil
Neutral salt spray, unlubricated, ASTM B11730 min≥ 10 h
Dry film thicknessmeasured per applicationmeasured per application
Shelf life, unopened, 5–35 °C12 months12 months

Both grades are supplied as a concentrate and diluted on site. Film thickness is set by dilution, part temperature and drain time, and is measured on your parts during the trial.

RHB-500

The wider process window: part entry up to 560 °C, bath up to 60 °C, curing from 80 °C. Built for shops that want the lowest conversion cost and do not carry a salt spray clause in the drawing.

RHB-3270

For drawings that specify salt spray. The unlubricated film reaches 10 hours or more to ASTM B117, which is a number you can put into a technical agreement. It needs an oven that holds 180–200 °C reliably.

Where it fits

Three production lines where the process already pays for itself

In each of these, the parts are hot when they leave the furnace, which is the only precondition that matters.

How we start

A trial on your line, not a data sheet argument

We send a 1 L sample of concentrate, which makes roughly 11 L of working bath. You run it on a batch of your own parts under your own furnace settings. That is the only test that settles anything, because film formation depends on part temperature and drain time in a way that a lab coupon cannot reproduce.

If the film covers evenly and the curing fits your oven, we quote on annual volume. If it does not, we say so and you have lost a sample, not a quarter.

  • 1 L sample of concentrate, shipped by air
  • Working dilution and bath make-up sheet
  • Technical data sheet and safety data sheet
  • Salt spray and film thickness measured on the trial parts
  • Volume pricing after the trial, not before

Questions

What buyers ask us first

Does RHB replace hot black oxide?

For parts that leave a tempering furnace hot, yes. It removes the caustic blackening bath, the preheat, the acid pickle and the rinse stages. For cold parts, or where the drawing calls for a conversion coating rather than an applied film, it is the wrong tool.

Is a drying oven still needed?

Yes. RHB-500 cures at 80–120 °C in forced air. RHB-3270 needs 180–200 °C for 3–5 minutes. Neither grade is a no-bake product.

What salt spray result can I put in a technical agreement?

Unlubricated film, ASTM B117: 30 minutes for RHB-500, 10 hours or more for RHB-3270. Both grades are oiled after blackening, and oiled performance is measured separately on your parts.

Which substrates are suitable?

Cast iron, carbon steel and powder-metallurgy parts. Not for aluminium or zinc-plated parts. Stainless steel needs an adhesion test before commercial use, because the passive chromium oxide layer resists organic films.

What does the bath need to be made up with?

RHB-500 dilutes with tap water at 1 : 10 or leaner. RHB-3270 needs deionised water below 200 µS/cm, because hardness ions interfere with the film on that grade.

How is it packaged for export?

5 US gal (18.9 L) pails and 55 US gal (208 L) drums. Transport classification is confirmed per shipment against the current transport assessment report.

Sample request

Tell us the part, the furnace and the drawing requirement

The three things that decide whether RHB fits are the part temperature on leaving the furnace, the curing temperature your line can hold, and whether the drawing carries a salt spray clause. Send those and we will answer with a grade, not a brochure.

Company
Dul Environmental Technology (Nanjing) Co., Ltd.
Address
Olympic Avenue 69, Jianye District, Nanjing, Jiangsu, China
Email
hongqi2222@126.com
Web
www.dulu-env.com