Residual Heat Blackening / Powder metallurgy

Application · Powder metallurgy

Black on PM parts, without committing the furnace to steam.

Steam treatment is the default black finish for sintered parts, and it earns its place: it seals surface porosity and it colours the part in the same pass. RHB separates those two jobs. Where the steam atmosphere is there for colour, a dip in residual heat does the colour and leaves the furnace free.

The distinction that decides it

Steam treatment does two things. Ask which one you are buying.

Steam is there for sealing

Steam at temperature oxidises the internal pore surfaces and closes them. That improves pressure tightness, corrosion resistance and, in many PM alloys, transverse strength. RHB does not do this. It forms a film on the outer surface and leaves the pore structure as it was. If sealing is the requirement, keep steam.

Steam is there for colour

Where the drawing just calls for a black finish and the part is oil-impregnated or painted afterwards anyway, the sealing value is partly redundant. That is the case where RHB makes sense: you get the colour from residual heat, and the furnace keeps running parts instead of oxidising atmospheres.

We will ask which of the two you need before quoting. If the answer is sealing, we will tell you to stay with steam treatment. That answer costs us an order and saves you a year of returns.

Process route

Where the heat comes from in a PM plant

1

Sinter

Parts leave the sintering furnace hot. Where a heat-treat or temper step follows, that discharge is the take-off point.

2

Temper

Parts must reach the bath at 200 °C or above. Below that, the film does not form, whatever the concentration.

3

Dip

30–60 seconds at 40–60 °C bath temperature, at 1 : 10 dilution. RHB-3270 requires deionised water below 200 µS/cm.

4

Cure and oil

80–120 °C forced air for RHB-500, or 180–200 °C for 3–5 minutes for RHB-3270. Oil while warm.

Oil impregnation is a separate operation and is not replaced by blackening. Sequence it after curing.

Comparison

Three routes, stated plainly

Steam treatmentHot black oxideRHB
Seals surface porosityYesNoNo
Black colourYes, blue-blackYesYes
Runs on residual heatUses furnace heatNo, needs a separate bathYes
Acid pickle requiredNoTypicalNo
Extra station after the furnaceNone, in-furnace42
Spent bath—Hot causticNear-neutral

This table is a process comparison, not a recommendation. The right route depends on which function the drawing actually specifies.

Next step

Send the part, the density and the drawing clause

For PM parts we also need the green density and whether the part is oil-impregnated, because both change how the film behaves at the pore edges. A 1 L sample makes about 11 L of working bath.