Application · Springs
A spring is a part held under permanent load. Anything that puts hydrogen into the surface is a fatigue risk you carry for the life of the part. RHB has no acid pickle and no electrolysis in the sequence: the part comes out of tempering hot and goes straight into a near-neutral bath.
The argument that matters
High-strength springs are the textbook case for hydrogen embrittlement. The risk enters through pickling, electroplating and cathodic cleaning — the steps that generate atomic hydrogen at the steel surface and let it diffuse inward.
Remove those steps and the route closes. RHB is applied to a hot part from a near-neutral aqueous bath, with no current and no acid. That does not make the finished spring embrittlement-proof, but it means blackening no longer adds a hydrogen source to a part that was previously clean.
Line fit
Compression, extension and torsion springs all run the same sequence. What changes between them is handling and fixturing at the dip, not the bath.
Tempering window
Spring tempering commonly lands in the 200–500 °C band, which is exactly the part entry temperature both grades are built for. RHB-3270 accepts up to 500 °C, RHB-500 up to 560 °C.
| Parameter | RHB-500 | RHB-3270 |
|---|---|---|
| Part entry temperature | 200–560 °C / 392–1040 °F | 200–500 °C / 392–932 °F |
| Bath temperature | 40–60 °C / 104–140 °F | 40–60 °C / 104–140 °F |
| Immersion time | 30–60 s | 30–60 s |
| Curing | 80–120 °C forced air | 180–200 °C, 3–5 min |
| Neutral salt spray, unlubricated, ASTM B117 | 30 min | ≥ 10 h |
Oil is applied after curing on both grades. Oiled performance is measured on your parts, not quoted from a table.
Honest limits